Analysis of several reasons for the deformation of two-color plastic molds?

Author: MULAN - Plastic Molding Manufacturer

Sometimes we will find that the two-color plastic mold products will be deformed. So do you know the reason why the two-color plastic mold products will be deformed? The following mold manufacturers will introduce to you. There are generally several reasons for the deformation of two-color plastic mold products.

1. Residual stress due to molding conditions; 2. Residual stress generated during demoulding; 3. Deformation due to lack of cooling time. 4. Residue caused by the shape of the product, especially the relationship between the forming shrinkage rate and the thickness of the product stress. Knowledge related to the deformation of two-color plastic mold products 1. The deformation of the product (warping, bending, small wrinkles) is the same as the cause of the crack. That is, the residual internal stress in the product.

The setting conditions for molding should be set in the direction of eliminating the internal stress of the product. That is, after increasing the barrel temperature and mold temperature, the injection pressure should not be too high when the material flow becomes better. 2. In order to reduce the residual internal stress, there is an annealing treatment, that is, the heat distortion temperature is below 10 degrees, and the heating for more than 2 hours can eliminate the internal stress.

However, this method of annealing is not widely used due to its high cost. 3. Assuming that the cooling water holes of the two-color plastic mold cannot uniformly cool the product, residual stress will also occur, which means that the cooling water holes should not be too shallow. If this happens, don’t panic, here we introduce the method of concentrated treatment 1. Immediately: fully cool and solidify in the mold (extend the cooling time timer), increase the temperature of the barrel, and reduce the injection pressure.

2. Short-term: Make the mold cooling uniform. 3. Long-term: To prevent the difference in product thickness, set the gate in the center of the product with large thickness. Because the straight line is easy to cause warping, a large R curve is made, and the mold with reversible bending of the product increases the number of ejector rods and increases the demoulding slope.

Mettiti in contatto con noi
Articoli raccomandati
BLOGS CASES
nessun dato

Cerchi una fabbrica di plastica in plastica affidabile e a svolta rapida di parti di plastica personalizzate? Con centinaia di macchinari di elaborazione, la nostra capacità interna senza pari garantisce che le tue parti vengano spedite puntuali, ogni volta. A Mulan Group, le nostre strutture certificate AS9100 sono progettate sia per la prototipazione rapida che per la produzione a basso volume di componenti di uso finale.

CONTACT US

Tel:86 21 3479 1660
Aggiungi: Building 37, 2049 Pujin Road, Pujiang, Minhang, Shanghai, Cina Chiamaci! Ottieni ora il tuo preventivo istantaneo!
Dal lunedì al venerdì: dalle 9 alle 18
Sabato:-Dunday: Chiudi
Diritto d'autore© 2025 Mulan Gruppo - www.china-plasticparts.com | Tutti i diritti riservati | Mappa del sito
Customer service
detect